Why Is Hot Melt Adhesive Stringing on Your Carton Sealing Line?

Find the cause of hot melt adhesive stringing on a carton sealer. Check nozzle position, cut-off, bead timing, temperature and board conditions.

Illustration of hot melt adhesive stringing between a dispensing nozzle and a corrugated carton flap on a sealing line

If thin adhesive threads follow each bead on your carton sealer, you are seeing hot melt adhesive stringing. Check the nozzle position and cut-off first.

Then verify bead placement, adhesive temperature at the applicator, and board conditions. Trial another grade only after these line variables are stable.

Stringing begins when molten adhesive fails to separate cleanly from the nozzle as a carton moves away. Turning up the tank temperature without checking the rest of the system can leave the cause unresolved and expose the adhesive to unnecessary heat.

Is the defect hot melt adhesive stringing or a dripping nozzle?

Stringing leaves a thin filament after a bead is dispensed; dripping leaves drops or continuing flow while the gun is closed. Watch several cycles at production speed and note which gun produces the defect. The visible pattern tells maintenance where to inspect first.

What you seeCheck firstWhy it matters
A thread follows the bead as the carton movesNozzle distance and cut-offAdhesive is stretching before it breaks from the tip.
Drops appear while the gun is closedValve module and nozzle tipFlow after shut-off points to a dispensing fault.
Glue trails beyond the flap edgeBead timing and lengthAdhesive outside the bond area can be pulled into a strand.
The problem starts after a board or shift changeBoard temperature and local airflowA changed surface or environment can alter bead behavior.

Is the nozzle too far from the carton?

Excessive distance gives the bead more room to stretch into a filament. Check the installed nozzle’s specified working distance and angle, particularly after a format change or nozzle replacement. Confirm that the carton passes the gun at a consistent height.

Bring the nozzle into its correct operating position according to the equipment manual. Keep the required clearance for moving cartons; a shorter gap helps only if the gun can still apply the bead reliably. For equipment-side checks, see Robatech’s guidance on avoiding hot melt stringing.

Is the bead ending beneath the flap?

The bead should stop inside the area that will be compressed between the flaps. Check the actual start and stop points on moving cartons, not only the programmed trigger settings. If adhesive runs beyond an edge, adjust the timing or bead length and check the finished seal.

Reducing the bead without checking bond coverage can exchange a stringing problem for an open carton. Keep the trial carton, board and line speed the same while evaluating the change.

Is the adhesive reaching the nozzle at its specified temperature?

Compare the tank, hose and applicator readings with the current adhesive data sheet and equipment instructions. A correct tank setting does not establish the temperature at the gun. Adhesive that cools on its way to the nozzle can become harder to cut off cleanly.

Check whether stringing appears after startup, a tank refill or a long idle period. Record the readings and the defect at each stage. Adjust temperatures only within the approved operating range; overheating can lead to adhesive degradation and equipment buildup.

Did the board or production environment change?

A colder board or direct airflow near the gun can change how quickly the bead cools. Compare board lots and storage conditions when stringing begins suddenly. Note nearby fans, air-conditioning outlets and open dock doors before changing the adhesive.

Run a controlled comparison with board held under normal production conditions. If the defect follows a particular board lot or shift, include that condition in any later adhesive trial.

When should you trial another adhesive?

Trial another grade when stringing persists after nozzle position, cut-off, bead timing and temperature are confirmed. Use the same board and machine settings for each candidate. Record visible threads and nozzle buildup, then verify that the carton still seals after compression and handling.

The packaging adhesive range is a starting point for selecting trial grades. For general-purpose corrugated cartons, the YD-5158 EVA carton sealing grade is one catalog candidate.

Ask for a current technical data sheet and assess clean cut-off alongside open time and bond performance. A bead that looks tidy is useful only if the sealed case also holds.

What should you send the supplier?

Send a short video showing the nozzle, bead and moving carton. Include the current adhesive and its data sheet, board type and storage conditions, line speed, nozzle model and position, and tank, hose and applicator readings. Note whether the defect occurs at startup, after refilling or throughout the shift.

These records give the supplier a basis for proposing a trial grade. They also help your team compare it with the current adhesive on the same line.

Inside Our Plant

Hot Melt Adhesive Made and Tested in Our Own Plant

See our factory and laboratory
Melt viscosity testing of yellow hot melt adhesive granules in the Good Adhesive laboratory

Tested in Our Own Laboratory

Grades are checked in our in-house laboratory, including melt viscosity, with more than 20 testing instruments.

Raw material storage for hot melt adhesive production at Good Adhesive

Controlled Raw Materials

Raw materials are stored on racked, labelled pallets in a dedicated warehouse before production.

Finished hot melt adhesive inventory on racked pallets ready to ship

Stock Ready to Ship

Finished hot melt adhesive is palletized in our warehouse, ready for export to 60+ countries.

Have a Question About Your Hot Melt Adhesive Line?

Send us your substrate, application method and line speed. Our engineers will recommend a grade and ship a free sample for testing.

Chat on WhatsApp
Free Sample · Technical Data Sheet

Request a Sample

Share the material, the line speed and the climate your product ships into. A sample and a technical data sheet follow from our export team.

Formulated to your substrate and line speed

Block, granule, flake, stick, powder or film

Factory-direct from Zhejiang to 60+ countries

Prefer to talk? WhatsApp +86 139 6713 4045 Tel +86-573-8884-9653

Phone: Mon–Fri, 9:30–17:30 China Time (GMT+8)

info@goodadhesive.com

Tell Us About Your Application

Fields marked * are required.